Abstract

In this research, a hybrid aluminum matrix nanocomposite was made using tungsten disulfide nanoparticles and carbon nanotube. Ultrasonic was used for mixing powders in acetone. Then hybrid particles and aluminum powder were mixed by mmechanical stirrer for 2 h and ball mill for 5h. The final mixed powder were compressed by hot pressing. Microstructural analysis of the specimens was performed by Optical Microscopy (OM) and Field Emission Scanning Electron Microscopy (FESEM). The results showed that the reinforcement phases were properly adsorbed on aluminum particles, there was a good distribution of the reinforcement particles in the aluminum matrix, and nanoparticles maintained their structure. The density of samples was measured by Archimedes method and the relative density of hybrid samples was found to be 96 to 98%. Micro hardness test showed that hybridization had a positive effect on the hardness and the hybrid nanocomposite micro hardness increased with increasing carbon nanotube content up to 20% that of Al/ WS2 nanocomposite. Compressive strength measurements showed that hybridization increased the final compressive strength up to 17%. Wear test showed the friction coefficient of the hybrid nanocomposite decreased up to 50% compared to the pure aluminum.

Keywords

[1] Yılmaz, O. and Buytoz, S. “Abrasive wear of Al2O3-reinforced aluminium-based MMCs”, Composites Science and Technology, vol. 61, pp. 2381-2392, 2001.
 [2] Feng, Y. Geng, L. Zheng, P. Zheng, Z. and Wang, G. “Fabrication and characteristic of Al-based hybrid composite reinforced with tungsten oxide particle and aluminum borate whisker by squeeze casting”, Materials & Design, vol. 29, pp. 2023-2026, 2008.
[3] Hu, Q. Luo, P.and Yan, Y. “Microstructures, densification and mechanical properties of TiC–Al2O3–Al composite by field-activated combustion synthesis”, Materials Science and Engineering: A, vol. 486, pp. 215-221, 2008.
[4] Alipour, M. and Eslami-Farsani, R., “Investigation of the microstructure and hardness of cast AA7068 nanocomposite reinforced with SiCnanoparticles”, In Persian, Journal of Science and Technology of Composites, Vol. 5, No. 4, pp. 461-468, 2019.
[5] Kumar, S. Chakraborty, M. Sarma, V. S. and Murty, B. “Tensile and wear behaviour of in situ Al–7Si/TiB2 particulate composites”, Wear, vol. 265, pp. 134-142, 2008.
[6] Gopalakrishnan, S.  and Murugan, N.  “Production and wear characterisation of AA 6061 matrix titanium carbide particulate reinforced composite by enhanced stir casting method”, Composites Part B: Engineering, vol. 43, pp. 302-308, 2012.
[7] Wozniak, J. Kostecki, M.  Cygan, T. Buczek, M. and Olszyna, A. “Self-lubricating aluminium matrix composites reinforced with 2D crystals”, Composites Part B: Engineering, vol. 111, pp. 1-9, 2017.
[8] Jirang, C. and Roven, H. J. “Recycling of automotive aluminum”, Transactions of Nonferrous Metals Society of China, vol. 20, pp. 2057-2063, 2010.
[9] Rengifo, S.  Zhang, C. Harimkar, S. Boesl, B. and Agarwal, A. “Effect of WS 2 Addition on Tribological Behavior of Aluminum at Room and Elevated Temperatures”, Tribology Letters, vol. 65, p. 76, 2017.
[10] Rajmohan, T. Palanikumar, K. and Ranganathan, S. “Evaluation of mechanical and wear properties of hybrid aluminium matrix composites”, Transactions of nonferrous metals society of China, vol. 23, pp. 2509-2517, 2013.
[11] Prasad, S. V. and Mecklenburg, K. R. “Self-lubricating aluminum metal-matrix composites”, Google Patents, 1996.
[12] Prasad, R. Asthan, A. “Aluminum metal-matrix composites for automotive applications tribological considerations”, Tribology Letters, vol17, pp 445–453, 2006.
[13] Jha, A. K. Dan, T. K. Prasad, S. V, Rohatgi, P. K. “Aluminum alloy solid lubricant talc particle composites”, Journal of Material Science, vol 21, pp 3681-3685, 1986 .
[14] Rajmohan, T. Palanikumar, K. “Modeling and analysis of Performance in drilling hybrid composites”, The International Journal of Advanced Manufacturing Technology, Vol 64, pp 1249–1261, 2013.
[15] Johny, S. Venkatesan, j. K. Kuppan, P. Ramanujam, R. “Hybrid Aluminium Metal Matrix Composite Reinforced with SiC and TiB2”, Procedia Engineering, vol 97, pp 1018 – 1026, 2014.
[16] Khani, M. Ezatpour, H. R. Ebrahimi, Gh. R. “Mechanical and microstructure properties of Al/CNT-Al2O3 hybrid nanocomposite produced by accumulative roll bonding process”, In Persian, Modares Mechanical Engineering, Vol. 17, No. 12, pp. 56-64, 2018 .
[17] Bodunrin, M. O. Alaneme, K. K. and Chown, L. H. “Aluminum matrix hybrid composites: a review of reinforcement philosophies; mechanical, corrosion and tribological characteristics”, Journal of materials research and technology, vol. 4, pp. 434-445, 2015.
[18] Muley, A. V. Aravindan, S.  and Singh, I. “Nano and hybrid aluminum based metal matrix composites: an overview”, Manufacturing Review, vol. 2, p. 15, 2015.
[19] Rikhtegar, F. Shabestari, S. and Saghafian, H. “Investigation of microstructure and mechanical properties of Al2024-CNT nanocomposite produced by flake powder metallurgy process”, In Persian, Journal of Science and Technology of Composites, Vol. 4, No. 1, pp. 91-100, 2017.
 [20] Bakshi, S. R. Lahiri, D. and Agarwal, A. “Carbon nanotube reinforced metal matrix composites-a review”, International materials reviews, vol. 55, pp. 41-64, 2010.
[21] Jam, j. m. Akbari, A. Khakbiz, M. “Fabrication Al6061/CNT Nanocomposite and Investigation of Wear Property” In Persian,  journal of advanced processes in material engineering, Vol 3, pp29-40, 2009. 
[22] Ahmed, Sh. Zayed, B. M. Kamel, T. A. Osman, O. A. Elkady, A. Shady, A. (2019) “Experimental study of tribological and mechanical properties of aluminum matrix reinforced by Al2O3/CNTs” Fullerenes, Nanotubes and Carbon Nanostructures in press DOI: 10.1080/1536383X.2019.1612882, 2019.
[23] Gowda, A. C. Girish, D. P. Santhosh, N. Kumar, A. “Study of Wear Characteristics of Aluminium/B4C/CNT Hybrid Composites under the Influence of Controlled Factors” Nano Trends: A Journal of Nanotechnology and Its Applications, Vol 18(2), pp 21-32, 2016.
[24] Huang, S.J. Ho, C.H. Feldman, Y. and Tenne, R. “Advanced AZ31 Mg alloy composites reinforced by WS2 nanotubes”, Journal of Alloys and Compounds, vol. 654, pp. 15-22, 2016.
[25] Huang, S.J. Lin, C.C. Huang, J.Y. and Tenne, R. “Mechanical behavior enhancement of AZ31/WS2 and AZ61/WS2 magnesium metal matrix nanocomposites”, Advances in Mechanical Engineering, vol. 10(2), pp. 1-14, 2018.
[26] Wang, Q. Chen, M. Shan, Z.  Sui, C. Zhang, L. Zhu, S. et al., “Comparative study of mechanical and wear behavior of Cu/WS2 composites fabricated by spark plasma sintering and hot pressing”, Journal of Materials Science & Technology, vol. 33, pp. 1416-1423, 2017.
 [27] Niste, V. B. Ratoi, M.  Tanaka, H.  Xu, F. Zhu, Y. and Sugimura, J.  “Self-lubricating Al-WS2 composites for efficient and greener tribological parts”, Scientific reports, vol. 7, p. 14665, 2017.
 [28] Vaziri, H. S. Shokuhfar, A. and Afghahi S. S.S. “Investigation of mechanical and tribological properties of aluminum reinforced with tungsten disulfide (WS2) nanoparticles”, Material. Research Express in press https://doi.org/10.1088/2053-1591/aafa00, 2018.
[29] Cavaliere, P.  Sadeghi, B. and Shabani A. “Carbon nanotube reinforced aluminum matrix composites produced by spark plasma sintering”, Journal of Materials Science, vol 52, pp 8618–8629, 2017.
[30] Shakeri, H.R. Wang, Z. “Effect of alternative aging process on the fracture and interfacial properties of particulate Al2O3–reinforced Al (6061) metal matrix  composite”, Metallurgical and Materials Transactions A, Vol. 33A, pp. 1699-1713, 2002.
 [31] Yarahmadi, A. Rajabi, M. Talafi Noghani, M. Taghiabadi, R. “Synthesis of Aluminum- CNTs Composites Using Double-Pressing Double-Sintering Method (DPDS)”, Nanostructure, vol 9(1), pp 94-102, 2019.